Heat transfer ink is printed onto release film by screen, dusted with hot-melt powder or over-printed with water-based adhesive, dried and gelled, then pressed onto fabric. The result sits thinner than plastisol with a silicone-like hand, suited to tag-less labels and high-stretch graphics.

Product range

ProductCode familyUse
Water-based colour ink1608 seriesClear, white, yellows, reds, violet, blue, green, black, silver, gold, specials
Screen printing colour ink2319 seriesScreen specific, balanced opacity and levelling
Anti-sublimation inkWMR series (black / white / clear)Blocks disperse dye migration on dark polyester blends
Two-component transfer inkW.S HT series (colour / white / anti-sublimation / clear)With hardener 1704 at 3%
Water-based adhesive7# adhesive, WS-HT900Adhesive layer by printing method
Hot-melt powder-Adhesive layer by powder method
AdditivesRetarder, thickener, hardener, silver paste, gold powderAdjust print behaviour

Printing parameters

InkMeshPassesNote
Colour ink90-120T1-2Next pass after surface drying
White ink68-90T2-4By opacity required
Anti-sublimation32-61T2-4By sublimation level of the fabric
Clear ink32T1Base layer for powder method

Process

  1. Mix 3% water-based hardener, stir well, use within pot life
  2. Screen print per the table, surface dry between passes
  3. Adhesive layer, one of two methods: powder - dust hot-melt powder while the clear ink is still wet; printing - print water-based adhesive through 24-32T, 2-3 passes after surface drying
  4. Dry at 70 C for 60 minutes, fully
  5. Gel in tunnel at 130 C
  6. Rest 24 hours before pressing and testing

Performance

ItemResult
Wash fastness60 C, 50 cycles, no cracking, no peeling, no staining (GB/T 8629)
ElasticityStretches 1.3-1.5 times without cracking
AbrasionAATCC 8 / ISO 105-X12, no rub-off, no staining
EnvironmentalWater-based, low VOC, low odour, no flash point

Suitable fabrics

Cotton, polyester, nylon, spandex and their blends, knitted and woven. Dark polyester-cotton without anti-sublimation treatment should be printed with the anti-sublimation ink first. Coated fabric, waterproof fabric and PU leather need a trial.

Common issues

  • Bubbling or poor adhesion - powder applied before the ink is fully dry, or insufficient resting time
  • Cracking - tested before the 24 hour rest, so the figures read low
  • Colour bleeding after wash - fabric not treated against sublimation, or adhesive layer too thin
  • Mesh clogging - ink not stirred, or shop temperature too high; add retarder

For a quotation: fabric composition and colour, print area, printing method, monthly volume, wash standard.

Frequently asked questions

What is WS-HT ink?

A water-based two-component heat transfer (heat transfer printing) ink, used for pattern transfer on garment fabrics.

How many washes does it withstand?

It withstands 50 washes at 60°C.

How many times can it stretch?

It stretches 1.3–1.5 times, suitable for pattern transfer on elastic fabrics.

What are the drying and powder-melting conditions?

Dry at 70°C × 60 minutes; powder melting temperature 130°C.

What is the difference from sublimation ink?

Sublimation ink relies on dye vaporization penetrating polyester fibers and is suitable for light-colored polyester; WS-HT is a pigment-based transfer ink with broader color coverage and application range, and can be used on cotton and blended fabrics.

Need the Specification Sheet?